SABIC Innovative Plastics LNP STAT-KON KE002 ACETAL

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON KE002 ACETAL.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* STAT-KON* KE002 is a compound based on Acetal resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.030 cm/cm

@Time 86400 sec
0.010 - 0.030 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 104 MPa
15100 psi
5 mm/min; ISO 527
106 MPa
15400 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 2.0 %
2.0 %
5 mm/min; ISO 527
2.4 %
2.4 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 8.22 GPa
1190 ksi
1 mm/min; ISO 527
Flexural Strength 154 MPa
22300 psi
ISO 178
161 MPa
23400 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 7.05 GPa
1020 ksi
2 mm/min; ISO 178
Izod Impact, Notched 0.420 J/cm
0.787 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.74 J/cm
7.01 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 161 °C
322 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
ASTM D257