SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+PS

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+PS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0045 - 0.0065 cm/cm

@Thickness 3.20 mm
0.0045 - 0.0065 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 15.3 g/10 min

@Load 5.00 kg,
Temperature 300 °C
15.3 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 106 MPa
15400 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 106 MPa
15400 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 2.5 %
2.5 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 2.5 %
2.5 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 20.68 GPa
2999 ksi
5 mm/min; ASTM D638
Flexural Strength 148 MPa
21500 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 15.85 GPa
2299 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.420 J/cm
0.787 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.76 J/cm
3.30 ft-lb/in
ASTM D4812
Dart Drop, Total Energy 9.00 J

@Temperature 23.0 °C
6.64 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 18.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 177 °C

@Thickness 3.20 mm
351 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 170 °C

@Thickness 3.20 mm
338 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 179 °C
354 °F
Rate B/50; ASTM D1525
Electrical Properties Metric English Comments
Surface Resistance 1000 ohm
1000 ohm
ASTM D257
Static Decay 0.010 sec
0.010 sec
5000V to <50V; FTMS101B
Copyright © lookpolymers.com All Rights Reserved