SABIC Innovative Plastics LNP STAT-KON ZX97172 PPE+PS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON ZX97172 PPE+PS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Electrically Conductive PPE+PS Blend Compound, containing a proprietary filler system.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0022 cm/cm
0.0022 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
5 mm/min; ISO 527
Elongation at Break 1.7 %
1.7 %
5 mm/min; ISO 527
Tensile Modulus 9.40 GPa
1360 ksi
1 mm/min; ISO 527
Flexural Modulus 7.10 GPa
1030 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 153 °C
307 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 147 °C
297 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 1000 ohm - 1e+05
1000 ohm - 1e+05
ROA; IEC 60093