Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-LOY NX03583 PC+ABS

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Stat-loy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-LOY NX03583 PC+ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP STAT-LOY* NX03583 is a compound based on PC+ABS Blend resin. Added features of this material include: Antistat, Flame Retardant.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 49.0 MPa
7110 psi
ASTM D638
Tensile Strength, Yield 56.0 MPa
8120 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Elongation at Yield 100 %
100 %
ASTM D638
Tensile Modulus 2.15 GPa
312 ksi
50 mm/min; ASTM D638
Flexural Strength 84.0 MPa
12200 psi
ASTM D790
Flexural Modulus 2.15 GPa
312 ksi
ASTM D790
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
Dart Drop, Total Energy 38.0 J
28.0 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C

@Thickness 3.20 mm
210 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0626 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Surface Resistance 1.00e+10 - 1.00e+12 ohm
1.00e+10 - 1.00e+12 ohm
ASTM D257
Users viewing this material also viewed the following: