Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-LOY P3000U PA 6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Stat-loy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-LOY P3000U PA 6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-loy* P3000U is a compound based on PA 6 resin. Added features include; Antistatic, UV - Stabilized.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ISO 1183
Water Absorption 6.3 %

@Time 86400 sec
6.3 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0080 cm/cm
0.0080 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.0 MPa
6380 psi
50 mm/min; ISO 527
Tensile Strength, Yield 56.0 MPa
8120 psi
50 mm/min; ISO 527
Elongation at Yield 3.6 %
3.6 %
50 mm/min; ISO 527
Flexural Yield Strength 59.0 MPa
8560 psi
2 mm/min; ISO 178
Flexural Modulus 1.80 GPa
261 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 162 °C
324 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 1.00e+10 - 1.00e+12 ohm
1.00e+10 - 1.00e+12 ohm
ASTM D257
Users viewing this material also viewed the following: