Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP AX06472 ABS

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP AX06472 ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* AX06472 is a compound based on ABS containing a clay blend.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Moisture Absorption 0.200 %
0.200 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Time 86400 sec
0.0040 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm

@Time 86400 sec
0.0050 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 2.0 %
2.0 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 5.93 GPa
860 ksi
50 mm/min; ASTM D638
Flexural Strength 96.0 MPa
13900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 5.38 GPa
780 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.420 J/cm
0.787 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.40 J/cm
4.50 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C

@Thickness 3.20 mm
205 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Dielectric Constant 3.0

@Frequency 1.00e+9 Hz
3.0

@Frequency 1.00e+9 Hz
ASTM D150
Dissipation Factor 0.0030

@Frequency 1.00e+9 Hz
0.0030

@Frequency 1.00e+9 Hz
ASTM D150
Users viewing this material also viewed the following: