SABIC Innovative Plastics LNP THERMOCOMP JF003E PES (Asia Pacific)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP JF003E PES (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* JF003E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
1.48 g/cc
0.0535 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 101 MPa
14600 psi
ASTM D638
Elongation at Break 2.3 %
2.3 %
ASTM D638
Tensile Modulus 5.95 GPa
863 ksi
50 mm/min; ASTM D638
Flexural Strength 158 MPa
22900 psi
ASTM D790
Flexural Modulus 5.81 GPa
843 ksi
ASTM D790
Izod Impact, Notched 0.420 J/cm
0.787 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.27 J/cm
8.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 207 °C

@Thickness 3.20 mm
405 °F

@Thickness 0.126 in
unannealed; ASTM D648