Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP MF006A PP (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP MF006A PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* MF006A is a compound based on Polypropylene resin containing Glass Fiber.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0012 cm/cm
0.0012 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 81.0 MPa
11700 psi
50 mm/min; ISO 527
Elongation at Yield 1.9 %
1.9 %
50 mm/min; ISO 527
Tensile Modulus 6.50 GPa
943 ksi
1 mm/min; ISO 527
Flexural Yield Strength 102 MPa
14800 psi
2 mm/min; ISO 178
Flexural Modulus 6.20 GPa
899 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 142 °C
288 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af