Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP OF008 PPS - Linear (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* OF008 is a compound based on PPS - Linear resin containing Glass Fiber.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0080 - 0.012 cm/cm

@Time 86400 sec
0.0080 - 0.012 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 159 MPa
23100 psi
5 mm/min; ISO 527
Elongation at Break 1.4 %
1.4 %
5 mm/min; ISO 527
Tensile Modulus 14.4 GPa
2090 ksi
1 mm/min; ISO 527
Flexural Strength 233 MPa
33800 psi
2 mm/min; ISO 178
Flexural Modulus 12.9 GPa
1870 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 14.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
7.78 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 45.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
25.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 278 °C
532 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
486 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af