SABIC Innovative Plastics LNP THERMOCOMP QF004 PA 6/10

Category Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP QF004 PA 6/10.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* QF004 is a compound based on Nylon 6/10 resin containing 20% Glass Fiber.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 111 MPa
16100 psi
ASTM D638
Elongation at Break 2.4 %
2.4 %
ASTM D638
Tensile Modulus 6.37 GPa
924 ksi
50 mm/min; ASTM D638
Flexural Strength 158 MPa
22900 psi
ASTM D790
Flexural Modulus 5.92 GPa
859 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.32 J/cm
8.09 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 203 °C

@Thickness 3.20 mm
397 °F

@Thickness 0.126 in
unannealed; ASTM D648