Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP RF006S PA6.6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP RF006S PA6.6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* RF006S is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 175 MPa
25400 psi
5 mm/min; ISO 527
Elongation at Break 2.0 - 4.0 %
2.0 - 4.0 %
5 mm/min; ISO 527
Tensile Modulus 9.50 GPa
1380 ksi
1 mm/min; ISO 527
Flexural Yield Strength 240 MPa
34800 psi
2 mm/min; ISO 178
Flexural Modulus 8.30 GPa
1200 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved