SABIC Innovative Plastics LNP THERMOCOMP UFW49S PPA (Asia Pacific)

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP UFW49S PPA (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* UFW49S is a compound based on Polyphthalamide resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized, Low Warpage.
Physical Properties Metric English Comments
Density 1.87 g/cc
0.0676 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0025 cm/cm

@Time 86400 sec
0.0025 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 192 MPa
27800 psi
ISO 527
Elongation at Break 1.1 %
1.1 %
ISO 527
Flexural Strength 274 MPa
39700 psi
ISO 178
Flexural Modulus 19.3 GPa
2800 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 37.0 kJ/m²
17.6 ft-lb/in²
80*10*4; ISO 180/1U