SABIC Innovative Plastics LNP THERMOCOMP UX93847 PPA (Asia Pacific)

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP UX93847 PPA (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* UX93847 is a compound based on Polyphthalamide resin containing Proprietary Filler(s).
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 192 MPa
27800 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 15.43 GPa
2238 ksi
50 mm/min; ASTM D638
Flexural Strength 296 MPa
42900 psi
ASTM D790
Flexural Modulus 12.84 GPa
1862 ksi
ASTM D790
Izod Impact, Notched 0.740 J/cm
1.39 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.93 J/cm
14.9 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 266 °C

@Thickness 3.20 mm
511 °F

@Thickness 0.126 in
unannealed; ASTM D648