Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP WX88406 Polyester, TP

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP WX88406 Polyester, TP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* WX88406 is a compound based on Polyester, TP resin.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 103 MPa
14900 psi
ASTM D638
103 MPa
14900 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 2.9 %
2.9 %
ASTM D638
2.9 %
2.9 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 7.92 GPa
1150 ksi
50 mm/min; ASTM D638
Flexural Strength 165 MPa
23900 psi
ASTM D790
165 MPa
23900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 7.06 GPa
1020 ksi
ASTM D790
7.06 GPa
1020 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.81 J/cm
12.8 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 202 °C

@Thickness 3.20 mm
396 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved