Material Notes:
LNP* Thermotuf* CF007IXP is a compound based on Polystyrene containing glass fiber. Characteristics of this grade are: High Impact.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Moisture Absorption 0.0500 %
0.0500 %
50% RH, 24 hrs; ASTM D570
0.0600 %
0.0600 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm

@Time 86400 sec
0.0010 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0030 - 0.0060 cm/cm

@Time 86400 sec
0.0030 - 0.0060 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.0 MPa
6380 psi
5 mm/min; ISO 527
50.0 MPa
7250 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 0.60 %
0.60 %
5 mm/min; ISO 527
0.70 %
0.70 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 8.91 GPa
1290 ksi
1 mm/min; ISO 527
10.23 GPa
1484 ksi
50 mm/min; ASTM D638
Flexural Strength 68.0 MPa
9860 psi
ISO 178
Flexural Yield Strength 71.0 MPa
10300 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 8.76 GPa
1270 ksi
2 mm/min; ISO 178
8.82 GPa
1280 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.30 J/cm
2.44 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 8.00 J

@Temperature 23.0 °C
5.90 ft-lb

@Temperature 73.4 °F
ASTM D3763
Impact Test 2.00 J
1.48 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 52.6 µm/m-°C

@Temperature -30.0 - 30.0 °C
29.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 53.3 µm/m-°C

@Temperature -30.0 - 30.0 °C
29.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
207 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
97.0 °C

@Thickness 3.20 mm
207 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
198 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
92.0 °C

@Thickness 3.20 mm
198 °F

@Thickness 0.126 in
unannealed; ASTM D648