Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOTUF OF008EI PPS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOTUF OF008EI PPS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermotuf* OF008EI is a compound based on PPS-Linear resin, containing Glass Fiber. Added features include : High Impact and Easy Molding.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0015 cm/cm
0.0015 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa
21000 psi
5 mm/min; ISO 527
Elongation at Break 1.8 %
1.8 %
5 mm/min; ISO 527
Tensile Modulus 12.5 GPa
1810 ksi
1 mm/min; ISO 527
Flexural Yield Strength 210 MPa
30500 psi
2 mm/min; ISO 178
Flexural Modulus 11.0 GPa
1600 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
19.0 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
8.33 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
26.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 263 °C
505 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af