Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOTUF W1000I PBT (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOTUF W1000I PBT (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOTUF* W1000I is a compound based on Polybutylene Terephalate resin. Added features include: High Impact
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Moisture Absorption 0.100 %
0.100 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.020 - 0.024 cm/cm
0.020 - 0.024 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.0 MPa
5220 psi
5 mm/min; ISO 527
Tensile Modulus 1.50 GPa
218 ksi
1 mm/min; ISO 527
Flexural Yield Strength 46.0 MPa
6670 psi
2 mm/min; ISO 178
Flexural Modulus 1.60 GPa
232 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 70.0 kJ/m²
33.3 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 140 µm/m-°C

@Temperature 23.0 - 60.0 °C
77.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 132 µm/m-°C

@Temperature 23.0 - 60.0 °C
73.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C
126 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
ASTM D257
Users viewing this material also viewed the following: