Material Notes:
LNP* Thermocomp* AF008 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 77.0 MPa
11200 psi
ASTM D 638
Elongation at Break 0.90 %
0.90 %
ASTM D 638
Tensile Modulus 11.99 GPa
1739 ksi
50 mm/min; ASTM D 638
Flexural Strength 117 MPa
17000 psi
ASTM D 790
Flexural Modulus 10.16 GPa
1474 ksi
ASTM D 790
Izod Impact, Notched 0.530 J/cm

@Temperature 23.0 °C
0.993 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 2.23 J/cm

@Temperature 23.0 °C
4.18 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 102 °C

@Thickness 3.20 mm
216 °F

@Thickness 0.126 in
unannealed; ASTM D 648