SABIC Innovative Plastics LNP Thermocomp OC004 PPS - Linear (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp OC004 PPS - Linear (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* OC004 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include : Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
Water Absorption 0.040 %

@Temperature 23.0 °C,
Time 86400 sec
0.040 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0015 cm/cm
0.0015 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 144 MPa
20900 psi
5 mm/min; ISO 527
Elongation at Break 1.1 %
1.1 %
5 mm/min; ISO 527
1.5 %
1.5 %
Flexural Strain, 2 mm/min; ISO 178
Tensile Modulus 16.6 GPa
2410 ksi
1 mm/min; ISO 527
Flexural Strength 193 MPa
28000 psi
2 mm/min; ISO 178
Flexural Yield Strength 194 MPa
28100 psi
2 mm/min; ISO 178
Flexural Modulus 15.1 GPa
2190 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
7.22 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 55.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
30.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 275 °C
527 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D 257