Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp PF006 PA 6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp PF006 PA 6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6 compound containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0090 - 0.013 cm/cm

@Time 86400 sec
0.0090 - 0.013 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 165 MPa
23900 psi
ISO 527
Elongation at Break 3.0 - 5.0 %
3.0 - 5.0 %
ISO 527
Tensile Modulus 8.50 GPa
1230 ksi
1 mm/min; ISO 527
Flexural Strength 225 MPa
32600 psi
ISO 178
Flexural Modulus 8.20 GPa
1190 ksi
ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 85.0 kJ/m²

@Temperature 23.0 °C
40.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 202 °C
396 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af