Material Notes:
LNP* Thermocomp* PZ006 is a compound based on Nylon 6 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.013 cm/cm

@Time 86400 sec
0.013 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 59.0 MPa
8560 psi
ASTM D 638
Elongation at Break 2.3 %
2.3 %
ASTM D 638
Tensile Modulus 5.12 GPa
743 ksi
50 mm/min; ASTM D 638
Flexural Strength 96.0 MPa
13900 psi
ASTM D 790
Flexural Modulus 3.86 GPa
560 ksi
ASTM D 790
Izod Impact, Notched 0.370 J/cm

@Temperature 23.0 °C
0.693 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 4.08 J/cm

@Temperature 23.0 °C
7.64 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812