Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermotuf VFM53 PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermotuf VFM53 PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOTUF* VFM53 is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 84.0 MPa
12200 psi
ASTM D 638
Elongation at Break 4.0 %
4.0 %
ASTM D 638
Flexural Strength 117 MPa
17000 psi
ASTM D 790
Flexural Modulus 3.41 GPa
495 ksi
ASTM D 790
Izod Impact, Notched 0.420 J/cm

@Temperature 23.0 °C
0.787 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Coefficient of Friction, Dynamic 0.75
0.75
ASTM D 3702 Modified
Coefficient of Friction, Static 0.55
0.55
ASTM D 3702 Modified
K (wear) Factor 207 x 10-8 mm³/N-M
103 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C

@Thickness 3.20 mm
185 °F

@Thickness 0.126 in
unannealed; ASTM D 648