SABIC Innovative Plastics LNP VERTON E9007E PEI

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON E9007E PEI.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* VERTON* E9007E is a compound based on Polyetherimide (PEI) containing 35% Long Carbon Fiber. Added features of this grade include: Structural, High Temperature
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 253 MPa
36700 psi
5 mm/min; ISO 527
267 MPa
38700 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 0.90 %
0.90 %
5 mm/min; ISO 527
1.0 %
1.0 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 32.0 GPa
4640 ksi
5 mm/min; ASTM D638
33.0 GPa
4790 ksi
1 mm/min; ISO 527
Flexural Strength 411 MPa
59600 psi
ISO 178
429 MPa
62200 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 28.5 GPa
4130 ksi
2 mm/min; ISO 178
28.9 GPa
4190 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.69 J/cm
3.17 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.20 J/cm
9.74 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 16.0 kJ/m²
7.61 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 34.0 kJ/m²
16.2 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 8.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
4.44 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 22.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
12.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af