SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Glass Fiber Filled , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
1.30 g/cc
0.0470 lb/in³
ISO 1183
Moisture Absorption 0.100 %
0.100 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 119 MPa
17300 psi
ASTM D638
124 MPa
18000 psi
ISO 527
Elongation at Break 2.1 %
2.1 %
ISO 527
2.4 %
2.4 %
ASTM D638
Tensile Modulus 6.61 GPa
959 ksi
50 mm/min; ASTM D638
7.79 GPa
1130 ksi
1 mm/min; ISO 527
Flexural Strength 139 MPa
20200 psi
ISO 178
159 MPa
23100 psi
ASTM D790
Flexural Modulus 5.67 GPa
822 ksi
ASTM D790
6.97 GPa
1010 ksi
ISO 178
Izod Impact, Notched 1.61 J/cm
3.02 ft-lb/in
ASTM D256
1.66 J/cm

@Temperature -40.0 °C
3.11 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Izod Impact, Unnotched 5.71 J/cm
10.7 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
80*10*4; ISO 180/1A
17.0 kJ/m²

@Temperature -40.0 °C
8.09 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 41.0 kJ/m²
19.5 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 16.0 J
11.8 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
44.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 46.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
47.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.5 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 133 °C

@Thickness 3.20 mm
271 °F

@Thickness 0.126 in
unannealed; ASTM D648