Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP VERTON RV007SX9 PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON RV007SX9 PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* VERTON* RV007SX9 is a compound based on PA 66 resin containing Long Glass Fiber.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Water Absorption 1.3 %

@Time 86400 sec
1.3 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0043 cm/cm

@Time 86400 sec
0.0043 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 195 MPa
28300 psi
5 mm/min; ISO 527
Elongation at Break 1.9 %
1.9 %
5 mm/min; ISO 527
Tensile Modulus 11.9 GPa
1730 ksi
1 mm/min; ISO 527
Flexural Strength 283 MPa
41000 psi
2 mm/min; ISO 178
Flexural Modulus 10.2 GPa
1480 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 52.0 kJ/m²
24.7 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 263 °C
505 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 259 °C
498 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
UL 94
Electrical Properties Metric English Comments
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
>= 120 arcs
UL 746A
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved