SABIC Innovative Plastics LNP VERTON RX00078 PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON RX00078 PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* VERTON* RX00078 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0022 cm/cm

@Time 86400 sec
0.0022 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0087 cm/cm

@Time 86400 sec
0.0087 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 197 MPa
28600 psi
5 mm/min; ISO 527
Elongation at Break 2.4 %
2.4 %
5 mm/min; ISO 527
Tensile Modulus 11.0 GPa
1600 ksi
1 mm/min; ISO 527
Flexural Strength 248 MPa
36000 psi
2 mm/min; ISO 178
Flexural Modulus 8.90 GPa
1290 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 70.0 kJ/m²
33.3 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
13.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 58.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
32.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 265 °C
509 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af