Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior applications (category R6). It also meets requirements of DIN5510-2, NFPA-130 and PN-K-02511 standards. Available in opaque colors.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
SABIC Method
Melt Flow 12 g/10 min

@Load 1.20 kg,
Temperature 300 °C
12 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Melt Index of Compound 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
Type I, 50 mm/min; ASTM D638
70.0 MPa
10200 psi
50 mm/min; ISO 527
Tensile Strength, Yield 77.0 MPa
11200 psi
Type I, 50 mm/min; ASTM D638
77.0 MPa
11200 psi
50 mm/min; ISO 527
Elongation at Break 80 %
80 %
Type I, 50 mm/min; ASTM D638
80 %
80 %
50 mm/min; ISO 527
Elongation at Yield 6.0 %
6.0 %
Type I, 50 mm/min; ASTM D638
6.0 %
6.0 %
50 mm/min; ISO 527
Tensile Modulus 2.60 GPa
377 ksi
5 mm/min; ASTM D638
2.60 GPa
377 ksi
1 mm/min; ISO 527
Flexural Yield Strength 110 MPa
16000 psi
2 mm/min; ISO 178
115 MPa
16700 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
1.3 mm/min, 50 mm span; ASTM D790
2.70 GPa
392 ksi
2 mm/min; ISO 178
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
0.900 J/cm

@Temperature -30.0 °C
1.69 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
80*10*4; ISO 180/1A
13.0 kJ/m²
6.19 ft-lb/in²
80*10*3; ISO 180/1A
6.00 kJ/m²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
10.0 kJ/m²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*3; ISO 180/1U
NB
NB
80*10*4; ISO 180/1U
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
80*10*3; ISO 180/1U
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched NB
NB
Edgew 80*10*3 sp=62mm; ISO 179/1eU
NB
NB
Edgew 80*10*4 sp=62mm; ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
1.40 J/cm²
6.66 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
Impact Test 125 J
92.2 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 60.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
60.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
60.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
104 °C

@Thickness 3.20 mm
219 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
93.0 °C

@Thickness 3.20 mm
199 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 114 °C
237 °F
Rate B/50; ISO 306
114 °C
237 °F
Rate B/50; ASTM D1525
115 °C
239 °F
Rate B/120; ISO 306
Descriptive Properties Value Comments
Fire Safety Hazard Level - Requirement set R6 HL3
EN EN 45545-2:2013
Heat release, MAHRE, 50 kW/m2, 3 mm <60kW/m^2
ISO 5660-1
Smoke density, DS-4, 50 kW/m2, 3mm <150
ISO 5659-2
Smoke density, VOF4, 50 kW/m2, 3mm <300
ISO 5659-2
Smoke toxicity, CITG (8 min), 50 kW/m2, 3 mm 0.1
ISO 5659-2