Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Lexan® FXD911A PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Lexan® FXD911A PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lexan FXD911A is a flame retardant, medium viscosity grade with release for the special effect appearance Diffusion in various colors. Color package may affect performance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.070 %
0.070 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %

@Temperature 23.0 °C
0.35 %

@Temperature 73.4 °F
ISO 62
Melt Flow 19 g/10 min

@Load 1.20 kg,
Temperature 300 °C
19 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 51.0 MPa
7400 psi
50 mm/min; ISO 527
Tensile Strength, Yield 63.0 MPa
9140 psi
50 mm/min; ISO 527
Elongation at Break 66.7 %
66.7 %
50 mm/min; ISO 527
Elongation at Yield 6.0 %
6.0 %
50 mm/min; ISO 527
Tensile Modulus 2.38 GPa
345 ksi
1 mm/min; ISO 527
Flexural Yield Strength 99.0 MPa
14400 psi
2 mm/min; ISO 178
Flexural Modulus 2.45 GPa
355 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
65.0 kJ/m²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
80*10*3; ISO 180/1U
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
6.50 J/cm²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 71.9 µm/m-°C

@Temperature 23.0 - 80.0 °C
39.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 69.6 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 141 °C
286 °F
Rate B/50; ISO 306
143 °C
289 °F
Rate B/120; ISO 306
Electrical Properties Metric English Comments
Dielectric Strength 23.4 kV/mm

@Thickness 3.20 mm
594 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
Comparative Tracking Index 200 V
200 V
IEC 60112
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2