Material Notes:
Lexan* R9453 Polycarbonate (PC) is a non-filled, non-chlorine and non-brominate flame retardant resin for general purpose, which contains 30% post-consumer recycled PC. This resin is of UL-94 V0 rating and for various injection molding applications. Limited availability and restricted color only.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0060 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.0 MPa
8410 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 64.0 MPa
9280 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 90 %
90 %
Type I, 50 mm/min; ASTM D638
Elongation at Yield 6.0 %
6.0 %
Type I, 50 mm/min; ASTM D638
Tensile Modulus 2.27 GPa
329 ksi
5 mm/min; ASTM D638
Flexural Yield Strength 87.0 MPa
12600 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 7.20 J/cm
13.5 ft-lb/in
ASTM D256
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 66.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 66.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 137 °C

@Thickness 3.20 mm
279 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 3.20 mm
259 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 145 °C
293 °F
Rate B/50; ASTM D1525
UL RTI, Electrical 130 °C
266 °F
UL 746B
UL RTI, Mechanical with Impact 120 °C
248 °F
UL 746B
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
Flammability, UL94 V-2

@Thickness 0.800 mm
V-2

@Thickness 0.0315 in
UL 94 by SABIC-IP
V-0

@Thickness 1.14 mm
V-0

@Thickness 0.0449 in
UL 94 by SABIC-IP
5VA

@Thickness 3.04 mm
5VA

@Thickness 0.120 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Arc Resistance 0.00 - 60 sec
0.00 - 60 sec
Tungsten; ASTM D495
Comparative Tracking Index 250 - 400 V
250 - 400 V
UL 746A
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
High Amp Arc Ignition, HAI 15 - 30 arcs
15 - 30 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min
>= 5.91 in/min
UL 746A