Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL CN5246 PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL CN5246 PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0025 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0025 - 0.0030 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 108 MPa
15700 psi
SABIC - Japan Method
Elongation at Break 7.0 %
7.0 %
SABIC - Japan Method
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 8.23 GPa
1190 ksi
ASTM D790
Izod Impact, Notched 0.680 J/cm
1.27 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 24.0 - 34.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
13.3 - 18.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 125 °C

@Thickness 6.40 mm
257 °F

@Thickness 0.252 in
unannealed; ASTM D648