Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL CN5260 PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL CN5260 PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
50% filled FR high modulus PPE/PS blend
Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0015 - 0.0025 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0025 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 13.3 g/10 min

@Load 5.00 kg,
Temperature 300 °C
13.3 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 129 MPa
18700 psi
SABIC - Japan Method
Elongation at Break 5.0 %
5.0 %
SABIC - Japan Method
Flexural Strength 161 MPa
23400 psi
ASTM D790
Flexural Modulus 12.35 GPa
1791 ksi
ASTM D790
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 20.0 - 31.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.1 - 17.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 125 °C

@Thickness 6.40 mm
257 °F

@Thickness 0.252 in
unannealed; ASTM D648
Users viewing this material also viewed the following: