Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL EM7301HF PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL EM7301HF PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Easy flow, 10% glass filled, improved adhesion PPO/HIPS alloy.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 71.0 MPa
10300 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 6.0 %
6.0 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 104 MPa
15100 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.59 GPa
521 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 112 °C

@Thickness 6.40 mm
234 °F

@Thickness 0.252 in
unannealed; ASTM D648
112 °C

@Thickness 3.20 mm
234 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: