Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL EN7010 PPE+SEBS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Styrene-Butadiene
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL EN7010 PPE+SEBS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High heat, Non halogenated flame retardant Noryl product for Film
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Viscosity 610000 cP
610000 cP
Melt Viscosity, 280°C, 1500 sec-1; ISO 11443
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 300 °C
12 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 71.0 MPa
10300 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 11 %
11 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 102 MPa
14800 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2.38 GPa
345 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 147 °C

@Thickness 6.40 mm
297 °F

@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 105 °C
221 °F
UL 746B
UL RTI, Mechanical with Impact 105 °C
221 °F
UL 746B
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Comparative Tracking Index 250 - 400 V
250 - 400 V
UL 746A
Users viewing this material also viewed the following: