Material Notes:
Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to allow for primer-less electrostatic painting. GTX679 has improved impact/elongation and the mineral content enables the material to be used in structural applications replacing metal or thermoset resins. The material is only available in black.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
Moisture Absorption 0.700 %
0.700 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 3.6 %
3.6 %
ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm

@Thickness 3.20 mm
0.0070 - 0.0090 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 16 g/10 min

@Load 5.00 kg,
Temperature 280 °C
16 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
Melt Index of Compound 14 g/10 min

@Load 5.00 kg,
Temperature 220 °C
14 g/10 min

@Load 11.0 lb,
Temperature 428 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 61.0 MPa
8850 psi
5 mm/min; ISO 527
62.0 MPa
8990 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 61.0 MPa
8850 psi
5 mm/min; ISO 527
64.0 MPa
9280 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type I, 5 mm/min; ASTM D638
5.0 %
5.0 %
5 mm/min; ISO 527
Elongation at Yield 2.0 %
2.0 %
5 mm/min; ISO 527
3.0 %
3.0 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 4.45 GPa
645 ksi
5 mm/min; ASTM D638
4.79 GPa
695 ksi
1 mm/min; ISO 527
Flexural Strength 108 MPa
15700 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Yield Strength 109 MPa
15800 psi
2 mm/min; ISO 178
Flexural Modulus 4.00 GPa
580 ksi
1.3 mm/min, 50 mm span; ASTM D790
4.44 GPa
644 ksi
2 mm/min; ISO 178
Izod Impact, Notched 0.390 J/cm
0.731 ft-lb/in
ASTM D256
0.310 J/cm

@Temperature -30.0 °C
0.581 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
3.00 kJ/m²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 7.00 J

@Temperature 23.0 °C
5.16 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 59.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
59.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 64.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
64.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
185 °C

@Thickness 3.20 mm
365 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 185 °C
365 °F
Rate B/50; ASTM D1525
185 °C
365 °F
Rate B/50; ISO 306
188 °C
370 °F
Rate B/120; ISO 306