Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL GTX GTX905 PPE+PS+PA

Category Polymer , Thermoplastic , Nylon , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GTX GTX905 PPE+PS+PA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Automotive.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.014 - 0.017 cm/cm
0.014 - 0.017 in/in
annealed 130C 1hr; ASTM D955
0.011 - 0.013 cm/cm

@Thickness 3.20 mm
0.011 - 0.013 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0090 - 0.012 cm/cm

@Thickness 3.20 mm
0.0090 - 0.012 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 8.0 g/10 min

@Load 5.00 kg,
Temperature 280 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 56.0 MPa
8120 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 49 %
49 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 87.0 MPa
12600 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 172 °C

@Thickness 6.40 mm
342 °F

@Thickness 0.252 in
unannealed; ASTM D648
Users viewing this material also viewed the following: