SABIC Innovative Plastics NORYL PX2956 PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL PX2956 PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE+PS GF+Mineral Filler total 35% FR V-0
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0030 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 15.5 g/10 min

@Load 5.00 kg,
Temperature 300 °C
15.5 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 126 MPa
18300 psi
SABIC - Japan Method
Elongation at Break 4.0 - 6.0 %
4.0 - 6.0 %
SABIC - Japan Method
Flexural Strength 154 MPa
22300 psi
ASTM D790
Flexural Modulus 8.43 GPa
1220 ksi
ASTM D790
Izod Impact, Notched 0.780 J/cm
1.46 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 22.0 - 34.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
12.2 - 18.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 125 °C

@Thickness 6.40 mm
257 °F

@Thickness 0.252 in
unannealed; ASTM D648