Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL WCP821U PPE-TPE (Asia Pacific)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL WCP821U PPE-TPE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV stabilized, halogen free Flexible Noryl injection molding grade for overmolding applications such as plugs, strain relief's, and connectors. Good color stability after UV weathering per ASTM D4459. Light color capable. UL94 V-0 performance with good processability.
Physical Properties Metric English Comments
Specific Gravity 1.05 - 1.12 g/cc
1.05 - 1.12 g/cc
ASTM D792
Water Absorption 0.10 %

@Time 173000 sec
0.10 %

@Time 48.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Time 86400 sec
0.0080 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.013 cm/cm

@Time 86400 sec
0.013 in/in

@Time 24.0 hour
ASTM D955
Melt Flow 14 g/10 min

@Load 2.16 kg,
Temperature 210 °C
14 g/10 min

@Load 4.76 lb,
Temperature 410 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
30S reading; ASTM D2240
Tensile Strength at Break 8.00 MPa
1160 psi
50 mm/min; ISO 527
9.00 MPa
1310 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 90 %
90 %
50 mm/min; ISO 527
95 %
95 %
Type I, 50 mm/min; ASTM D638
Flexural Modulus 0.130 GPa
18.9 ksi
12.5 mm/min, 100 mm span; ASTM D790
0.170 GPa
24.7 ksi
12.5 mm/min; ISO 178
Thermal Properties Metric English Comments
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
UL 94
HB

@Thickness 1.00 mm
HB

@Thickness 0.0394 in
UL 94
V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
UL 94
Oxygen Index 25 %
25 %
ISO 4589
Glow Wire Test 725 °C
1340 °F
IEC 60695-2-13
750 °C

@Thickness 3.00 mm
1380 °F

@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 3.40e+15 ohm-cm
3.40e+15 ohm-cm
ASTM D257
Dielectric Constant 2.7

@Frequency 1.00e+6 Hz
2.7

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 24.5 kV/mm

@Thickness 2.00 mm
622 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
Dissipation Factor 0.0040

@Frequency 1.00e+6 Hz
0.0040

@Frequency 1.00e+6 Hz
ASTM D150
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Smoke Density on 0.5mm plaque, Flame, Ds, max 126
ASTM E 662
Smoke Density on 0.5mm plaque, Non-flame, Ds, max 147
ASTM E 662