Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Noryl V080 PPE+HIPS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NORYL V080 is an unfilled, flame retardant, high flow material and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
on tensile bar; SABIC Method
Melt Flow 25 g/10 min

@Load 1.20 kg,
Temperature 280 °C
25 g/10 min

@Load 2.65 lb,
Temperature 536 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
Tensile Strength at Break 35.0 MPa
5080 psi
50 mm/min; ISO 527
Tensile Strength, Yield 40.0 MPa
5800 psi
50 mm/min; ISO 527
Elongation at Break 20 %
20 %
50 mm/min; ISO 527
Elongation at Yield 3.0 %
3.0 %
50 mm/min; ISO 527
Tensile Modulus 2.10 GPa
305 ksi
1 mm/min; ISO 527
Flexural Yield Strength 60.0 MPa
8700 psi
2 mm/min; ISO 178
Flexural Modulus 2.25 GPa
326 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
40.0 kJ/m²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 80.0 °C
176 °F
Rate B/50; ISO 306
82.0 °C
180 °F
Rate B/120; ISO 306
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
UL 94
V-0

@Thickness 2.50 mm
V-0

@Thickness 0.0984 in
UL 94
Oxygen Index 32 %
32 %
LOI; ISO 4589
Glow Wire Test 960 °C

@Thickness 3.20 mm
1760 °F

@Thickness 0.126 in
Glow Wire Flammability Index; IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ROA; IEC 60093
Dielectric Constant 2.6

@Frequency 1.00e+6 Hz
2.6

@Frequency 1.00e+6 Hz
IEC 60250
2.7

@Frequency 50.0 - 60.0 Hz
2.7

@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 18.0 kV/mm

@Thickness 3.20 mm
457 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
Dissipation Factor 0.0040

@Frequency 1.00e+6 Hz
0.0040

@Frequency 1.00e+6 Hz
IEC 60250
0.010

@Frequency 50.0 - 60.0 Hz
0.010

@Frequency 50.0 - 60.0 Hz
IEC 60250