Material Notes:
45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.
Physical Properties Metric English Comments
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0015 - 0.0025 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0025 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 4.6 g/10 min

@Load 6.60 kg,
Temperature 337 °C
4.6 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 131 MPa
19000 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 1.4 %
1.4 %
Type I, 5 mm/min; ASTM D638
Flexural Strength 179 MPa
26000 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 12.41 GPa
1800 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
2.18 J/cm

@Thickness 3.20 mm
4.08 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 212 °C

@Thickness 6.40 mm
414 °F

@Thickness 0.252 in
unannealed; ASTM D648
Glass Transition Temp, Tg 217 °C
423 °F
UL RTI, Electrical 180 °C
356 °F
UL 746B
UL RTI, Mechanical with Impact 180 °C
356 °F
UL 746B
UL RTI, Mechanical without Impact 180 °C
356 °F
UL 746B
Flammability, UL94 V-0

@Thickness 0.780 mm
V-0

@Thickness 0.0307 in
UL 94
5VA

@Thickness 2.99 mm
5VA

@Thickness 0.118 in
UL 94
Electrical Properties Metric English Comments
Arc Resistance 120 - 180 sec
120 - 180 sec
Tungsten; ASTM D495
Comparative Tracking Index 100 - 175 V
100 - 175 V
UL 746A
Hot Wire Ignition, HWI 60 - 120 sec
60 - 120 sec
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
0.00 - 15 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min
>= 5.91 in/min
UL 746A
Users viewing this material also viewed the following: