SABIC Innovative Plastics ULTEM Foam XP080 PEI

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name ULTEM Foam
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics ULTEM Foam XP080 PEI.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The foam also possesses excellent dielectric properties. ULTEM foam is targeted at applications where structural fire performance, radar transparency, or extreme hot or cold environments are required. ULTEM foam is thermoformable and compatible with phenolic pre-pregs. Information on processing or secondary operations is available upon request.
Physical Properties Metric English Comments
Density 0.0800 g/cc
0.00289 lb/in³
ASTM D1622
Water Absorption 4.0 %
4.0 %
ASTM C272
Mechanical Properties Metric English Comments
Tensile Strength 1.70 MPa
247 psi
ASTM D638
Tensile Modulus 0.0370 GPa
5.37 ksi
in plane; ASTM D638
Compressive Strength 1.20 MPa
174 psi
perpendicular to plane; ASTM D1621
Compressive Modulus 0.0710 GPa
10.3 ksi
ASTM D1621
Shear Modulus 0.0190 GPa
2.76 ksi
ASTM C273
Shear Strength 1.00 MPa
145 psi
ASTM C273
Izod Impact, Unnotched (ISO) 0.800 kJ/m²
0.381 ft-lb/in²
ISO R179
Thermal Properties Metric English Comments
Thermal Conductivity 0.0370 W/m-K
0.257 BTU-in/hr-ft²-°F
ASTM C518
Descriptive Properties Value Comments
Insulation Radiant Panel PASSES
FAR 25.856
OSU total heat release (2 minute test) <55kW-min/m^2
FAR 25.853
OSU peak heat release rate (5 minute test) <55kW/m^2
FAR 25.853
Smoke Density <10Ds
FAR 25.853
Smoke Toxicity PASSES
OEM BSS
PASSES
OEM ABD
Vertical Burn at 60 Seconds PASSES
FAR 25.853