Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Xenoy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Xenoy® FXX210SK PBT+PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
XENOY FXX210SK is an unreinforced PBT+PC injection moulding resin with excellent impact characteristics and containing a metal sparkle Visual FX. Applications: automotive bezels and appliances. XENOY FXX210SK is the visual FX version of XENOY CL100.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 250 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 482 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
50 mm/min; ISO 527
Elongation at Break 60 %
60 %
50 mm/min; ISO 527
Tensile Modulus 2.25 GPa
326 ksi
1 mm/min; ISO 527
Izod Impact, Unnotched (ISO) 32.0 kJ/m²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Vicat Softening Point 115 °C
239 °F
Rate B/120; ISO 306