Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC PP 526P Polypropylene Homopolymer for Cast Film

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer SABIC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC PP 526P Polypropylene Homopolymer for Cast Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: PP 526P is specially developed for cast film applications for producing clear films and does not contain slip or antiblock additives.Films produced using PP 526P will exhibit:Consistent processabilityHigh gloss and clarityGood melt strengthGood mechanical propertiesFilm produced can be metalizedTypical Applications: PP 526P can be used for producing fool and non-food packaging, stationary items and films for DVD casings for label insertion.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102
102
ASTM D785
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus, 1% Secant 1650 MPa
239000 psi
ASTM D790A
Izod Impact, Notched 0.250 J/cm
0.468 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Vicat Softening Point 152 °C
306 °F
ASTM D1525B
Processing Properties Metric English Comments
Processing Temperature 210 - 250 °C
410 - 482 °F
Barrel Temperature
Copyright © lookpolymers.com All Rights Reserved