Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC PP 57MNK10 Polypropylene Impact Copolymer for Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer SABIC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC PP 57MNK10 Polypropylene Impact Copolymer for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: PP 57MNK10 is a controlled rheology PP grade of medium molecular weight distribution specially developed for producing injection molded articles. This grade has an excellent impact resistance (even at low temperature) and good stiffness.Typical Applications: PP 57MNK10 can be used for garden furniture, housewares, containers, toys, crates and boxes.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 - 0.025 cm/cm
0.012 - 0.025 in/in
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ASTM D785
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus, 1% Secant 1300 MPa
189000 psi
ASTM D790A
Izod Impact, Notched 0.550 J/cm

@Temperature -20.0 °C
1.03 ft-lb/in

@Temperature -4.00 °F
ASTM D256
1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525B
Processing Properties Metric English Comments
Processing Temperature 200 - 240 °C
392 - 464 °F
Barrel Temperature
Mold Temperature 15.0 - 40.0 °C
59.0 - 104 °F