Material Notes:
Product Description: PP 623B is a PP Random Copolymer grade specially designed for Cast PP (CPP) film extrusion. It contains slip agent and anti-block additives. PP 623B offers good heat weldability for the sealing layers of CPP film.Films produced using PP 623B will exhibit:Excellent processabilityGood weldabilityHigh clarityHigh gloss.Typical Applications: PP 623B can be used mainly for cast film food and non-food packaging.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 92
92
ASTM D785
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus, 1% Secant 950 MPa
138000 psi
ASTM D790A
Izod Impact, Notched 0.550 J/cm
1.03 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C
172 °F
ASTM D648
Vicat Softening Point 132 °C
270 °F
ASTM D1525B
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved