Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC R50035 Linear Low Density Polyethylene for Rotational Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Manufacturer SABIC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC R50035 Linear Low Density Polyethylene for Rotational Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: R50035 are Linear Low Density Polyethylene grades designed to provide excellent stress crack resistance, mechanical properties with high rigidity, toughness, gloss and low warpage.R50035 Series includes the following grades:R50035: Non UV stabilized, PelletsR50035E: UV stabilized, PelletsRG50035: Non UV stabilized, PowderTypical Applications: Rotational molding of large industrial and agricultural tanks, trash containers and chemical shipping drums. They are also suitable for injection molding applications like caps, closures and housewares. RG50035 is suitable for producing compounds & masterbatches.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 150 hour
>= 150 hour
F50; ASTM D1693B
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength at Break 17.0 MPa
2470 psi
ASTM D638
Tensile Strength, Yield 16.0 MPa
2320 psi
ASTM D638
Elongation at Break 590 %
590 %
ASTM D638
Flexural Strength 13.0 MPa
1890 psi
ASTM D790
1% Secant Modulus 420 MPa
60900 psi
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 114 °C
237 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746