Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SCG Chemicals EL-Leneâ„¢ H5211PBL High Density Polyethylene Pipe Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer SCG Chemicals Co.
Trade Name EL-Lene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SCG Chemicals EL-Leneâ„¢ H5211PBL High Density Polyethylene Pipe Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE80 pipe, non pressure pipesCertification: Certified by LNEInformation provided by SCG Chemicals
Physical Properties Metric English Comments
Specific Gravity 0.956 g/cc
0.956 g/cc
ISO 1183
Environmental Stress Crack Resistance >= 10000 hour
>= 10000 hour
F0; ASTM D1693
Oxidative Induction Time (OIT) >= 20 min

@Temperature 200 °C
>= 20 min

@Temperature 392 °F
ISO/TR10837
Melt Flow 0.44 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.44 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength at Break 35.0 MPa
5080 psi
Crosshead speed 100 mm/min; ISO 527
Tensile Strength, Yield 25.0 MPa
3630 psi
Crosshead speed 100 mm/min; ISO 527
Elongation at Break 860 %
860 %
Crosshead speed 100 mm/min; ISO 527
Flexural Modulus 1.08 GPa
157 ksi
ASTM D790
Izod Impact, Notched 1.74 J/cm

@Temperature 23.0 °C
3.25 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746
Descriptive Properties Value Comments
Carbon Black/Pigment Dispersion (grade) <3
ISO 18553
Color Blue
RAL5012