S&E Specialty Polymers CPE-01-266A-405 Black PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer S&E Specialty Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers CPE-01-266A-405 Black PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: 90° C, oil resistant CPE based, FT4, 210,000 BTU wire and cable jacketing material with enhanced tear properties and flexibility.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.35 - 1.41 g/cc
1.35 - 1.41 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90 - 95
90 - 95
ASTM D2240
Tensile Strength 12.4 MPa
1800 psi
ASTM D412
13.46 MPa

@Treatment Temp. 121 °C,
Time 605000 sec
1952 psi

@Treatment Temp. 250 °F,
Time 168 hour
Air Oven aged; UL1581
Elongation at Break 325 %
325 %
ASTM D412
390 %

@Treatment Temp. 121 °C,
Time 605000 sec
390 %

@Treatment Temp. 250 °F,
Time 168 hour
Air Oven aged; UL1581
Thermal Properties Metric English Comments
Brittleness Temperature <= -16.0 °C
<= 3.20 °F
ASTM D746
Oxygen Index 36 %
36 %
ASTM D2863