S&E Specialty Polymers GA-1042LF PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GA-1042LF PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: UL bulletinized PVC based compound, suitable for injection molding application.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.38 g/cc
1.32 - 1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90 - 94
90 - 94
ASTM D2240
Tensile Strength 18.3 MPa
2650 psi
ASTM D412
20.13 MPa

@Treatment Temp. 136 °C,
Time 605000 sec
2920 psi

@Treatment Temp. 277 °F,
Time 168 hour
Air Oven aged
Elongation at Break 310 %
310 %
ASTM D412
251.1 %

@Treatment Temp. 136 °C,
Time 605000 sec
251.1 %

@Treatment Temp. 277 °F,
Time 168 hour
Air Oven aged
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -18.0 °C
-0.400 °F
ASTM D746
Oxygen Index 26 %
26 %
ASTM D2863