S&E Specialty Polymers TufPrene™ 2000-40 SEBS

Category Polymer , Thermoplastic , Styrene-Butadiene , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer S&E Specialty Polymers
Trade Name TufPrene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufPrene™ 2000-40 SEBS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: TufPrene 2000-40 is a member of our “unfilled” standard SEBS product line, which ranges from 30 to 90 Shore A. It is a general purpose material designed primarily for injection molding. Modifications are available on a custom basis for extrusion or other processes.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Melt Flow 30.0 g/10 min

@Load 4.90 kg,
Temperature 200 °C
30.0 g/10 min

@Load 10.8 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 41.0
41.0
ASTM D2240
Tensile Strength 5.38 MPa
780 psi
ASTM D412
Elongation at Break 873 %
873 %
Ultimate; ASTM D412
100% Modulus 0.000848 GPa
0.123 ksi
ASTM D412
Tear Strength 18.6 kN/m
106 pli
ASTM D624
Compression Set 13.0 %
13.0 %
ASTM D395-B