S&E Specialty Polymers TufTech™ GA-3174 PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufTech™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufTech™ GA-3174 PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: 80°C PVC General Purpose Jacketing compound with high gloss surface.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 73.0

@Time 15.0 sec
73.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 12.4 MPa
1800 psi
ASTM D412
Elongation at Break 300 %
300 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -29.0 °C
-20.2 °F
ASTM D746
Oxygen Index 24.0 %
24.0 %
ASTM D2863
Processing Properties Metric English Comments
Processing Temperature 171 - 177 °C
340 - 350 °F
Suggested Stock